Silk Screen Glass Definition
Silk screen glass is made by printing ceramic paint through a stencil mesh onto the glass surface, then tempering the glass. The paint fuses into the glass, becoming permanent and weather-resistant.
Key Features
Durable and fade-resistant pattern
Anti-glare and shading properties
Custom patterns: dots, stripes, gradients, logos
Enhanced visual and functional design
Applications
Sunshade panels and glass louvres
Spandrel glass in facades
Elevator cabins and partitions
Storefronts and public signage
Interior decoration and furniture
Subtypes
Tempered silk screen glass
Laminated silk screen glass
Insulated silk screen glass
Custom pattern options (frit dots, lines, logo printing)
Category | Parameter | Standard Example | Technical Notes |
Basic Properties | Glass Type | Clear Tempered, Ultra-Clear, Low-E Coated, Patterned, Curved | Customizable colors, patterns, and coatings |
| Thickness Range (mm) | 4~19 (Common: 5/6/8/10/12/15/19) | Thickness tolerance: ±0.2mm (GB 15763.2) |
Mechanical Performance | Surface Compressive Stress (MPa) | ≥95 (Standard) | Heat-Strengthened: 24~69 MPa |
≥150 (High-Strength) |
| Bending Strength (MPa) | 3~5x Annealed Glass | Test method: ASTM C1048 |
(5mm: ≥70; 8mm: ≥90) |
| Impact Resistance (Steel Ball) | 5mm: 1040g ball @ 1m height (no break) | Complies with GB 17841 safety requirements |
10mm: 2270g ball @ 2m (EN 12600) |
Safety Features | Fragmentation Pattern | 40~400 fragments in 50×50mm area (5mm) | Crumbles into granular pieces with blunt edges |
Max. fragment weight: ≤0.5g (GB 15763.2) |
| Thermal Shock Resistance (ΔT) | Withstands ≥220°C (e.g., 300°C → room temperature) | No cracks (Test per GB 15763.2) |
Optical Properties | Light Transmittance (%) | Clear: ≥89% (4mm) | Low-E coating adjusts transmittance to 50%~80% |
Ultra-Clear: ≥91% (6mm) |
| UV Blocking Rate (%) | Clear: <60 | Depends on coating type |
Low-E: ≥90 |
Dimensions | Min. Size | 300×300 mm | Most sizes customizable
|
Max. Size | 3300×13000 mm |
| Minimum Hole/Notch Margin | Edge distance ≥2×glass thickness (e.g., 5mm glass → ≥10mm) | Prevents edge stress concentration |
Heating Stage | Furnace Temperature (°C) | 700~720 (near softening point) | Heating time: 40~60 sec/mm (≤6mm), 60~80 sec/mm (≥8mm) |
Quenching Stage | Cooling Air Pressure (%) | 4mm: 95~100% | Rapid cooling induces surface compressive stress |
10mm: 85~90% |
Edge Treatment | Grinding/Polishing | CNC precision grinding (R-angle ≤0.5mm) | Reduces spontaneous breakage risk |
Mirror/matte finish |
Special Treatment | Heat Soak Test (HST) | 290°C±10°C for ≥2 hours (reduces NiS-induced breakage) | Lowers breakage rate from 0.3% to <0.1% (GB 15763.2) |
Application | Recommended Configuration | Certifications |
Building Facades | 8~12mm clear/ultra-clear, U-value ≤1.8 | EN 12150, ASTM C1048, GB 15763.2 |
Furniture/Partitions | 5~8mm patterned/frosted, fragment count ≥40 | CNS 11227 (Taiwan), JIS R3205 (Japan) |
Automotive Side Windows | 4~5mm curved, visible light transmittance ≥70% (GB 9656) | ECE R43, ISO 3537 |
Solar Panels | 3.2~4mm ultra-clear textured, transmittance ≥91.5% | IEC 61215 (UV/thermal cycling tests) |